生產防火板時候容易出現(xiàn)三個問題
來源:http://www.xamgdj.com/ 日期:2022-10-21 發(fā)布人:admin
富美家防火板的耐熱、耐磨、耐刮、耐感染、抗沖擊、防水等各項性能相對與其他的表面裝飾材料有突出的優(yōu)勢,所以在市場中的購買前景不錯,下面就來講講生產防火板時候容易出現(xiàn)三個問題,做好預防措施。
The heat resistance, abrasion resistance, scratch resistance, infection resistance, impact resistance, water resistance and other properties of Fumeijia fire-proof board have outstanding advantages compared with other surface decoration materials, so the purchase prospect in the market is good. Now let's talk about three problems that are easy to occur in the production of fire-proof board, and take preventive measures.
一、板面局部有白花
1、 There are some white flowers on the board surface
產生的原因:
Causes:
1、表層紙含膠量不足或干燥中局部樹脂固化
1. Insufficient glue content of surface paper or partial resin curing during drying
2、表層紙揮發(fā)物含量過低
2. The volatile content of surface paper is too low
3、熱壓式壓力不均勻
3. Uneven hot pressing pressure
4、忖墊材料無彈性
4. The cushion material is inelastic
5、不銹鋼板表明不平
5. Stainless steel plate indicates unevenness
6、樹脂反應過老,分子太大,樹脂流動性大
6. The resin reaction is too old, the molecule is too large, and the resin fluidity is large
解決的方法:
Solution:
1、提高表層紙樹脂含量或控制干燥溫度,防止局部樹脂固化
1. Increase resin content of surface paper or control drying temperature to prevent local resin solidification
2、提高表層紙的揮發(fā)物含量
2. Improve the volatile content of surface paper
3、檢修熱壓機,改進加壓面的均勻性
3. Overhaul the hot press and improve the uniformity of the pressure surface
4、定期更換忖墊材料
4. Replace the cushion material regularly
5、不銹鋼板定期拋光
5. Regular polishing of stainless steel plate
6、樹脂應分析檢驗,不合格指標要求時停止使用
6. The resin shall be analyzed and inspected, and it shall not be used when it is unqualified
在生產防火板的過程中易出現(xiàn)的問題
Problems easy to occur in the production of fireproof boards
二、板面有濕花(水汽),邊緣較為嚴重
2、 There are wet streaks (moisture) on the board surface, and the edges are relatively serious
產生的原因:
Causes:
1、浸膠紙干燥后揮發(fā)物含量太高
1. The volatile content of the impregnated paper is too high after drying
2、印刷木紋的油墨或染料所用的溶劑不合適
2. The solvent used for printing wood grain ink or dye is inappropriate
3、浸膠干燥后的膠膜紙吸濕(回潮)
3. Moisture absorption (moisture regain) of impregnated and dried adhesive film paper
解決的方法:
Solution:
1、降低浸膠紙干燥后的揮發(fā)物含量
1. Reducing Volatile Content of Dried Impregnated Paper
2、調換油墨(染料)用的溶劑
2. Solvent for changing ink (dye)
3、注意膠膜紙的存放,一般可用塑料布遮蓋
3. Pay attention to the storage of adhesive film paper, which can generally be covered with plastic cloth
在生產防火板的過程中易出現(xiàn)的問題
Problems easy to occur in the production of fireproof boards


三、裝飾板表面開裂
3、 The surface of the decorative plate is cracked
產生的原因:
Causes:
1、樹脂反應過嫩,分子太小
1. The resin is too tender and the molecule is too small
2、樹脂固化不完全
2. Incomplete resin curing
3、表層膠膜紙含膠量太高
3. The adhesive content of the surface adhesive film paper is too high
解決的方法:
Solution:
1、不合格的樹脂停止使用
1. Unqualified resin shall not be used
2、適當提高熱壓溫度或延長熱壓時間
2. Properly increase the hot pressing temperature or extend the hot pressing time
3、控制表層膠膜紙的含膠量
3. Control the glue content of the surface adhesive film paper
生產防火板時候容易出現(xiàn)三個問題就是以上所講解的內容了,您對此有什么想咨詢的地方或者有采購需求,都可以來我們網站http://www.xamgdj.com看看。
There are three problems that are easy to occur in the production of fireproof boards. If you have any questions or purchase needs, you can come to our website http://www.xamgdj.com have a look.
上一篇:如何檢驗優(yōu)良裝飾材料抗倍特板材?
下一篇:抗倍特掛墻板的基本安裝步驟
Related products相關新聞
- 酒店餐飲選材避坑!富美家防火板實測,阻燃耐磨雙在線,10...2026-04-25
- 別瞎選富美家HPL!6種常規(guī)厚度實測,甲方指定款+場景適...2026-04-18
- 避坑!墻面裝飾板選不對虧大了,富美家防火板憑實力碾壓,適...2026-04-13
- 富美家裝飾耐火板:千色百紋的HPL飾面美學全解析2026-04-07
- 早刷到這篇文章就好了,家里富美家室內門就不會踩坑了2026-04-06
- 富美家室內門怎么選?從幾百元到兩三千,它們之間的差距是啥...2026-03-18
- 富美家衛(wèi)生間隔斷,別忽略3個易壞配件!選對省大錢2026-03-16
- 富美家抗倍特有什么實力?2026-03-11
- 富美家衛(wèi)生間隔斷全解析:為何防火板復合防潮基層方案是性價...2026-03-03
- 裝修選板避坑!富美家不燃板,顏值與硬實力雙在線才靠譜2026-02-21
山東創(chuàng)圖建筑裝飾工程有限公司


13953117233
您當前位置:


產品銷售熱線:13953117233
技術方案咨詢:18560211715 18663705616
倉庫地址:山東省濟南市天橋區(qū)金鑫產業(yè)園303倉庫